Lalacewar daya: Ba za a iya zuba ba
Siffofin: siffar simintin gyare-gyare ba ta cika ba, gefuna da sasanninta suna zagaye, waɗanda aka fi gani a sassa na bango na bakin ciki.
Dalilai:
1. Ruwan oxygen na baƙin ƙarfe yana da tsanani, carbon da silicon abun ciki yana da ƙasa, abun ciki na sulfur yana da girma;
.
Hanyoyin rigakafin:
1. Bincika ko girman iskar ya yi yawa;
2. Ƙara relay coke, daidaita tsayin coke na kasa;
3. Inganta zafin simintin ɗimbin yawa da saurin yin simintin, kuma kar a yanke magudanar ruwa yayin simintin.
Laifi na biyu: raguwa sako-sako
Siffofin: farfajiya na pores yana da m kuma ba daidai ba, tare da lu'ulu'u na dendritic, ƙananan pores don shrinkage, ƙananan tarwatsawa don raguwa, ya fi kowa a cikin nodes masu zafi.
Dalilai:
1. Abubuwan da ke cikin carbon da silicon sun yi ƙasa sosai, raguwa yana da girma, ciyarwar mai tashi bai isa ba;
2. Zazzabi mai zafi yana da yawa kuma raguwa yana da girma;
3, Rigar wuyan yayi tsayi da yawa, sashe yayi karami;
4, yawan zafin jiki na simintin gyare-gyare ya yi ƙasa da ƙasa, rashin ruwa mara kyau na baƙin ƙarfe, yana shafar ciyarwa;
Hanyoyin rigakafin:
1. Sarrafa nau'in sinadarai na ƙwayar ƙarfe don hana ƙananan carbon da silicon abun ciki;
2. Tsananin sarrafa yawan zafin jiki;
3, m zane riser, idan ya cancanta, tare da sanyi baƙin ƙarfe, don tabbatar da jerin solidification;
4. Ƙara abun ciki na bismuth daidai.
Lalabi uku: zafi mai zafi, fashewar sanyi
Fasaloli: Tsatsa mai zafi shine karaya tare da iyakar hatsi a babban zafin jiki, tare da siffa mai banƙyama da launi mai oxidizing. Zafafan zafi na ciki yakan kasance tare tare da rami mai raguwa.
Cold crack yana faruwa a ƙananan zafin jiki, karaya mai jujjuyawa, siffa mai lebur, ƙyalli na ƙarfe ko ƙasa mai oxidized.
Dalilai:
1, solidification tsari shrinkage an katange;
2, Abubuwan da ke cikin carbon a cikin ƙarfe na ruwa ya yi ƙasa da ƙasa, abin da ke cikin sulfur ya yi yawa, kuma yawan zafin jiki ya yi yawa;
3, abun ciki na baƙin ƙarfe ruwa yana da girma;
4. Abubuwan hadaddun an cika su da wuri.
Hanyoyin rigakafin:
1, inganta nau'in, ainihin rangwame;
2. Yawan adadin carbon kada ya zama ƙasa da 2.3%;
3, sarrafa abun ciki na sulfur;
4, cupola zuwa cikakken tanda, girman iska ba zai iya zama babba ba;
5, guje wa yawan zafin jiki na simintin gyare-gyare, kuma inganta saurin sanyi, don tace hatsi;
6. Sarrafa marufi zazzabi.